2.2 The heat resistance of the coating is extremely sensitive to water. In humid environments, heat resistance decreases significantly. The thermal decomposition temperature in the dry environment is 130 ° C, and the thermal decomposition temperature in the humid environment is only 60 ° C, which leads to the limited use environment of chlorinated rubber coating, and the maximum use environment temperature cannot exceed 70 ° C.


 

Meistä

Yrityksemmehas always been adhering to the "'science and technology, quality first, honest and trustworthy , strictimplementation of ls0900l:.2000 international quality management system.Our rigorous managementtechnologicdinnovation, quality service cast the quality of products, won the recognition of the majority of users .Ammattitaito- ja vahvana kiinalaisena tehtaalla